伴随着冬的到来,天气将越来越寒冷,对于彩钢瓦翻新修缮来说,也将面临着喷漆干燥时间延长,原装漆上被冻了,漆膜容易开裂,雨露打花漆膜,温度差等等一系列问题。那么济南彩钢瓦翻新修缮过程中要注意什么?
With the arrival of the winter solstice, the weather will get colder and colder. For the renovation and repair of color steel tiles, there will also be a series of problems such as extended drying time of paint spraying, frozen original paint, easy cracking of paint film, rain and dew scratching paint film, temperature difference, etc. So what should we pay attention to in the process of renovation and repair of Jinan color steel tiles?
1.需要在施工前提前了解天气情况。由于漆膜需要充分的干燥时间,一般来说,彩钢瓦的翻新修缮基本上都是在室外进行,如果施工前忽略了对天气情况的提前了解,一旦遇上雨雪天气,将会造成工期延期或者未干的漆膜受损等情况,进而影响施工的品质和时间。
1. It is necessary to know the weather conditions in advance before construction. As the paint film needs sufficient drying time, generally speaking, the renovation and repair of color steel tiles are basically carried out outdoors. If the weather conditions are ignored before construction, the construction period will be delayed or the wet paint film will be damaged in case of rain and snow, which will affect the quality and time of construction.
2.如果在冬天施工,还要注意露水、霜冻等天气情况,以避免发生漆膜还没干透便被露水侵蚀,造成漆膜被水迹弄花。通常情况而言,由于水性彩钢瓦翻新专用漆,以水为溶剂的特点,彩钢翻新漆工程施工时的环境温度不低于10摄氏度,自然环境空气相对湿度不大于60%,在10℃以下的翻新喷漆工程中,必须采用加温的方法。
2. If the construction is carried out in winter, pay attention to the weather conditions such as dew and frost, so as to prevent the paint film from being eroded by dew before it is completely dry, causing the paint film to be stained by water. Generally speaking, due to the special water-based paint for refurbishment of color steel tiles, which uses water as the solvent, the ambient temperature during the construction of the color steel refurbishment paint project is not less than 10 ℃, and the relative humidity of the natural ambient air is not more than 60%. In the refurbishment paint project below 10 ℃, the heating method must be used.、
济南彩钢
3.彩钢瓦翻新喷漆前必须要对屋面整体进行打磨处理,掉残留的焊渣、旧起皮、浮锈等,打磨完毕后再彻底的冲洗一下屋面,将打磨产生的碎屑冲干净,为喷涂底漆作准备。
3. Before color steel tile renovation and painting, the whole roof must be polished to remove the residual welding slag, old peeling, floating rust, etc. After polishing, the roof shall be thoroughly washed to clean the debris generated by polishing to prepare for painting primer.
4.在彩钢瓦翻新修缮的施工过程中,须将彩钢瓦翻新专用漆进行多遍喷涂,需要注意的是,一定要等到上一道涂层彻底干透后再喷涂下一道工序,否则很容易造成漆膜脱落、起泡等现象的发生后,水性彩钢瓦翻新专用漆喷涂时千万不能往里面加入油漆类的稀释剂。
4. During the construction of renovation and repair of color steel tiles, the special paint for renovation of color steel tiles must be sprayed for many times. It should be noted that the next process must be sprayed after the previous coating is completely dry, otherwise it is easy to cause paint film falling off, blistering and other phenomena. When spraying the special paint for renovation of water-based color steel tiles, paint thinners must not be added.
在进行喷漆前要注意查看彩钢瓦的锈蚀情况,再根据屋面具体情况制定一个合理的施工方案,以确保工程质量。而在彩钢瓦翻新修缮的过程中,细节才是决定施工品质的保证。更多相关内容就来我们网站http://www.lxcaigang.com咨询吧!
Before painting, pay attention to the corrosion of color steel tiles, and then formulate a reasonable construction plan according to the specific conditions of the roof to ensure the project quality. In the process of renovation and repair of color steel tiles, details are the guarantee of construction quality. More relevant content will come to our website http://www.lxcaigang.com Consult!