 不管在建筑行业、造船行业、家具行业、电气行业中都离不开彩钢板,但同时彩钢板的发展也正在不断地进行创新,虽彩钢板的性能很好,但在特殊情况下偶尔也会出现部分问题。而彩钢板“爆漆”现象就是比较常见的,今天济南彩钢板房的小编给大家解析彩钢板爆漆的原因
  No matter in the construction industry, shipbuilding industry, furniture industry, electrical industry are inseparable from color steel plate, but at the same time, the development of color steel plate is also constantly innovative. Although the performance of color steel plate is very good, some problems will occasionally appear in special cases. And color steel plate "paint" phenomenon is more common, today's Jinan color steel panel room for everyone to analyze the causes of color steel plate paint explosion
  1、配槽过程中,要加钝化液后加水,因为钝化液密度问题,会导致原料混合不均匀,从而会出现钝化层与基板附着力差,让彩钢板表面出现爆漆现象。
  1. In the process of tank preparation, water should be added after adding passivation solution. Due to the density of passivation solution, raw materials will be mixed unevenly, resulting in poor adhesion between the passivation layer and the substrate, resulting in paint explosion on the surface of color steel plate.
 
  2、化板温生茶工艺规定为2h一次,主要因为相关作业人员没有定时对钝化板温度进行跟踪。特别在冬季,2h内的温度变化很大,从而会导致彩钢板失效,在压型时会出现因划伤而掉漆的现象。
  2. The chemical plate temperature raw tea process is required to be once every 2 hours, mainly because the relevant operators did not regularly track the temperature of the passivation plate. Especially in winter, the temperature changes greatly within 2 hours, which will lead to the failure of color steel plate and the phenomenon of paint dropping due to scratch during molding.
  3、生产彩钢板过程中,出口检查镜上有灰尘,部分棍子同样有灰尘的存在。而灰尘会直接影响彩钢板表面质量,起初不会表现出来,但经过长时间的使用或经过阳光的暴晒后,就会出现爆漆现象。
  3. During the production of color steel plate, there is dust on the exit inspection mirror, and some sticks also have dust. Dust will directly affect the surface quality of color steel plate, which will not show at first, but after a long time of use or after exposure to the sun, the phenomenon of paint explosion will appear.
  以上便是彩钢板出现爆漆的三种情况,我们在平时一定要注意这些问题,正确合理的存放和使用彩钢板,从而避免爆漆现象。想要了解更多内容欢迎咨询济南彩钢板房http://www.lxcaigang.com官网。
  The above are the three cases of paint explosion on color steel plate. We must pay attention to these problems at ordinary times, store and use color steel plate correctly and reasonably, so as to avoid paint explosion. For more information, welcome to consult Jinan color steel panel roomhttp://www.lxcaigang.com Official website.